COOLTHERM EP 6972 KIT
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- <0.0005 ohm-cm Volume Resistivity
- 2.13 W/(m K) Thermal Conductivity
- 1:1 Weight Mixing
Product Description
CoolTherm EP-6972 Conductive Adhesive is a two-part, silver-filled epoxy adhesive for electrically and thermally conductive bonding. Resin and hardener mix 1:1 by weight for manual or automatic meter/mix/dispense application. Cure schedules are 40 minutes at 85 deg C or 20 minutes at 100 deg C after the material reaches the target temperature. Typical cured properties include volume resistivity below 0.0005 ohm-cm and thermal conductivity of 2.13 W/(m K). The stated service-temperature range is -50 to +150 deg C.
Key features
- Cured volume resistivity: Typical cured value is below 0.0005 ohm-cm at 25 deg C using ASTM D257.
- Cured thermal conductivity: Typical cured thermal conductivity is 2.13 W/(m K).
- Equal-ratio weight mixing: Resin and hardener mix 1:1 by weight before application.
Applications
General circuit board repair; conductive bonding where electrical and thermal conductivity are required.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Resin and hardener are supplied as separate components; mixed values apply after the 1:1 by-weight mix.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Mix ratio, resin:hardener | 1:1 | by weight | Before application |
| Specific gravity, resin | 3.49 | Typical; resin | |
| Specific gravity, hardener | 3.55 | Typical; hardener | |
| Specific gravity, mixed | 3.52 | Typical; mixed material | |
| Working life | >1 | h | Typical; mixed material; 25 deg C; 100 g mass |
Cured adhesive properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Volume resistivity | <0.0005 | ohm-cm | Typical; ASTM D257; 25 deg C |
| Thermal conductivity | 2.13 | W/(m K) | Typical |
| Hardness | 80 | Shore D | Typical |
| Lap shear strength | 1200 | psi | Typical; aluminum-to-aluminum |