3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a white, flame-retardant two-part epoxy for metal and composite honeycomb structures, insert bonding, and aircraft-interior panels. Mix Part B and Part A at 100:50 by volume; the thixotropic paste resists sagging and provides more than 60 minutes of work life at 22 deg C. Full cure is achieved in 24 hours at 24 deg C or one hour at 82 deg C. The cured adhesive reaches 5000 psi aluminum overlap shear and meets the stated 14 CFR 25.853(a) flammability requirements before and after environmental conditioning.
Key features
- Flame Retardant Interior Bonding: The cured adhesive meets the stated 14 CFR 25.853(a) flammability requirements.
- Non Sag Honeycomb Placement: Thixotropic paste controls application in panels, inserts, and vertical joints.
- Extended Assembly Work Life: More than 60 minutes supports dispensing, positioning, and fixture setup.
Applications
Aircraft-interior honeycomb panels, insert bonding, galleys, luggage bins, partitions, lavatories, seating structures, and sidewall panels.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Part B color | White | - | Before mixing |
| Part A color | Gray | - | Before mixing |
| Mix ratio by weight | 100:40 | B:A | Two-part system |
| Mix ratio by volume | 100:50 | B:A | Two-part system |
| Solids | 100 | % | Both components |
| Consistency | Thixotropic paste | - | Mixed adhesive |
| Work life | More than 60 | min | At 22 deg C |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | - | Cured |
| Density | 1.3 | g/cm3 | Cured; typical |
| Volatile loss on cure | Less than 0.1 | % | Cured adhesive |
| Overlap shear strength | 5000 | psi | Aluminum; ASTM D1002; tested at 24 deg C |
| Floating roller peel strength | 33 | piw | Aluminum with EW-5000 primer; ASTM D3167 at 24 deg C |
| Tensile strength | 8200 | psi | ASTM D638; controlled heat cure |
| Elongation at break | 3.4 | % | ASTM D638; controlled heat cure |