3M CV45F

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M CV45F

Main features

  • Conformable Panel Seam Bonding
  • Immediate Pressure Sensitive Handling
  • Stress Relaxing Acrylic Foam

Product Description

3M VHB Commercial Vehicle Tape CV45F is a gray, conformable double-sided acrylic foam tape for commercial-vehicle panel-to-panel attachment at overlap seams. The 1.1 mm viscoelastic foam construction bonds on contact and provides immediate handling strength with firm application pressure. Its acrylic chemistry supports stress relaxation, environmental durability, and differential movement between compatible panels. CV45F bonds common vehicle materials including bare and painted metals and fiberglass-reinforced plastic when the surfaces and joint design follow the specified application process.

Key features

  • Conformable Panel Seam Bonding: The 1.1 mm foam tape supports commercial-vehicle panel overlap seams.
  • Immediate Pressure Sensitive Handling: The acrylic adhesive bonds on contact after firm application pressure.
  • Stress Relaxing Acrylic Foam: The viscoelastic core absorbs energy and accommodates differential panel movement.

Applications

Commercial-vehicle panel overlap seams, roof-panel attachment, side-panel bonding, and compatible trim assembly.

Product Family

3M CV45F

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Gray | Red
DensityDensity
720 kg/m3
Total ThicknessTotal Thickness
1100 μm
Other Properties
Storage TemperatureStorage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorGray-As supplied
Adhesive typeMultipurpose acrylic-Double-sided tape
Foam typeConformable acrylic foam-Viscoelastic core
Density720kg/m3ASTM D3574; foam with adhesive
Total tape thickness1.1mmASTM D3652
Release linerPE film-Red liner
Liner thickness0.13mmNominal
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
90 deg peel adhesion44N/cmASTM D3330; aluminum; 72 h at 23 deg C; 304 mm/min
Normal tensile strength585kPaASTM D897; aluminum; 72 h at 23 deg C
Overlap shear strength480kPaASTM D1002; stainless steel; 72 h at 23 deg C
Short-duration temperature resistance149deg CFour-hour conditioning
Long-duration temperature resistance93deg CStatic shear for 10000 min

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch