3M 9472

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 9472

Main features

  • High Tack Transfer Bonding
  • Converter Friendly Fiber Reinforcement
  • Broad Substrate Peel Performance

Product Description

3M Adhesive Transfer Tape 9472 uses fibered Adhesive 300 on a tan densified kraft release liner to support thin, high-tack attachment. The 5 mil tape construction provides conformability for graphic overlays, metal nameplates, rating plates, and foam lamination. Pressure-sensitive bonding develops with firm application pressure, while adhesion continues to build after assembly. Performance data covers common substrates including ABS, polypropylene, and stainless steel under controlled peel conditions. The liner protects the adhesive during converting and can support die-cut parts before final placement.

Key features

  • Fibered Acrylic Adhesive: Adhesive 300 combines high tack with handling support for converting.
  • Five Mil Tape Construction: The thin adhesive layer supports overlays, nameplates, and foam laminations.
  • Broad Substrate Adhesion: Qualified peel data covers ABS, polypropylene, and stainless steel surfaces.

Applications

Graphic overlays, metal nameplates, rating plates, and foam lamination for gasket fabrication.

Product Family

3M 9472

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Tan
Total ThicknessTotal Thickness
130 μm
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Adhesive typeFibered acrylic Adhesive 300-As supplied
Total tape thickness5milNominal
Release liner60 lb densified kraft-Tan liner
Liner thickness3.5milNominal
ColorTan-Liner appearance
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Peel adhesion on ABS4.4N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Peel adhesion on polypropylene6.8N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Peel adhesion on stainless steel9.4N/cm90 deg peel after 72 h at 23 deg C; 2 mil aluminum backing; 304 mm/min
Short-duration temperature resistance121deg CMinutes to hours
Long-duration temperature resistance70deg CDays to weeks

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol