3M 898

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 898

Main features

  • High-Tensile Filament Reinforcement
  • Multi-Surface Synthetic-Rubber Adhesion
  • Consistent Curl-Resistant Dispensing

Product Description

Scotch Filament Tape 898 is a clear filament-reinforced polypropylene tape with a multi-layer synthetic-rubber adhesive system for high-strength reinforcement and heavy-duty strapping. The 0.168 mm construction combines glass yarn filaments with a backing that resists nicks, abrasion, moisture, scuffing, and breakage, even when nicked or punctured. Its adhesive bonds to corrugated cardboard, fiberboard, plastics, metals, and oily surfaces, and the tape is engineered to dispense consistently without curling. The reinforced construction is intended for demanding packaging, shipment reinforcement, bundling, and strapping work.

Key features

  • High-tensile filament reinforcement: Glass yarn reinforcement provides long-term holding power and high tensile strength for demanding packaging loads.
  • Multi-surface synthetic-rubber adhesion: The adhesive system bonds to corrugated cardboard, fiberboard, plastics, metals, and oily surfaces.
  • Durable controlled dispensing: The reinforced backing resists abrasion and moisture while the roll dispenses consistently without curling.

Applications

Applications include full-overlap L-clip box closures, metal and pipe bundling, large bulk-container reinforcement, high-strength reinforcement, and heavy-duty strapping.

Product Family

3M 898

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Clear
Total ThicknessTotal Thickness
170 μm
Mechanical Properties
ElongationElongation
5 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
665 N/cm
Other Properties
Storage TemperatureStorage Temperature
4 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingPolypropylene filmClear filament-reinforced construction
Fiber reinforcementGlass yarnAs supplied
Adhesive systemMulti-layer synthetic rubberPressure-sensitive
Total tape thickness0.168mmTypical
Product colorTransparentAs supplied

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers